Print

周金柱:航空轮胎排气孔漏气原因分析及改进措施论文

本文主要研究内容

作者周金柱,祁跃猛,宁永刚,王宇宸,王轶(2019)在《航空轮胎排气孔漏气原因分析及改进措施》一文中研究指出:分析航空轮胎使用过程中排气孔漏气的原因,并提出改进措施。由胎体排气造成的漏气不会降低轮胎充气压力,为正常现象;由橡胶透气性造成的漏气会略降低轮胎充气压力,但过程非常缓慢,为正常现象;由胎里露线或其他原因导致帘线与胎腔内的高压气体直接接触造成的漏气,轮胎充气压力下降较快,影响使用。通过改进气密层胶配方,严格工艺操作规程和加强半成品检测可减少排气孔漏气现象发生。

Abstract

fen xi hang kong lun tai shi yong guo cheng zhong pai qi kong lou qi de yuan yin ,bing di chu gai jin cuo shi 。you tai ti pai qi zao cheng de lou qi bu hui jiang di lun tai chong qi ya li ,wei zheng chang xian xiang ;you xiang jiao tou qi xing zao cheng de lou qi hui lve jiang di lun tai chong qi ya li ,dan guo cheng fei chang huan man ,wei zheng chang xian xiang ;you tai li lou xian huo ji ta yuan yin dao zhi lian xian yu tai qiang nei de gao ya qi ti zhi jie jie chu zao cheng de lou qi ,lun tai chong qi ya li xia jiang jiao kuai ,ying xiang shi yong 。tong guo gai jin qi mi ceng jiao pei fang ,yan ge gong yi cao zuo gui cheng he jia jiang ban cheng pin jian ce ke jian shao pai qi kong lou qi xian xiang fa sheng 。

论文参考文献

  • [1].航空轮胎常见故障研究[J]. 赵安家,孟哲理.  飞机设计.2019(03)
  • [2].硬脂酸锌在解决无内胎航空轮胎胎里裂口中的应用研究[J]. 湛瑞芳,李文胜,常浩,孟向阳.  现代橡胶技术.2014(03)
  • [3].我国自主研发军用航空轮胎试用成功[J].   塑料制造.2015(08)
  • [4].我国军用航空轮胎材料将国产化[J]. 中新.  军民两用技术与产品.2015(15)
  • [5].我军用航空轮胎材料将实现国产化[J]. 新型.  化工新型材料.2015(11)
  • [6].2013航空轮胎标准化年会圆满落幕[J]. 关泰.  橡塑技术与装备.2013(11)
  • [7].米其林计划关闭航空轮胎厂[J]. 冯涛.  轮胎工业.2010(07)
  • [8].航空轮胎工业正向子午化发展[J]. 李汉堂.  现代橡胶技术.2010(06)
  • [9].航空轮胎标准化技术委员会召开第四届二次工作会议[J]. 张萍.  现代橡胶技术.2008(03)
  • [10].米其林第300万条航空轮胎下线[J]. 钱伯章.  橡胶科技市场.2008(20)
  • 论文详细介绍

    论文作者分别是来自轮胎工业的周金柱,祁跃猛,宁永刚,王宇宸,王轶,发表于刊物轮胎工业2019年10期论文,是一篇关于航空轮胎论文,排气孔论文,漏气论文,原因分析论文,气密层论文,轮胎工业2019年10期论文的文章。本文可供学术参考使用,各位学者可以免费参考阅读下载,文章观点不代表本站观点,资料来自轮胎工业2019年10期论文网站,若本站收录的文献无意侵犯了您的著作版权,请联系我们删除。